Di Noer Checks Titanium Plates Before MMO Coating: Racking And Thread Caps Reviewed
Nov 18, 2026

Report A batch of Grade 2 titanium plates completed pretreatment and moved to the pre-coating racking check at the coating workshop, the shop said. Operators worked from both sides of a vertical multi-tier rack, checking the blue protective caps on the conductive threaded studs piece by piece, along with the plate faces for knocks and the tiers for hard contact. The batch then went on to thermal-decomposition coating.
Before coating, the plates pass through degreasing, grit blasting, acid activation, deionized-water rinsing and drying, staff said. The blast board for this batch records Ra 3.5–5 μm with 60–80 mesh white alumina - the shop's own window. Titanium forms a passive film in air; pretreatment removes that film and the machining residue and leaves a rough surface for mechanical anchoring. Rougher is not automatically better, since over-blasting damages thin plate dimensions.
The rack is a vertical multi-tier frame. Plates sit one per tier, conductive studs pointing up, each capped in blue. Working down the tiers, the operators confirm caps are seated, plate edges are free of chips, and pieces are not touching. The conductive contact section is kept out of the coating step - a boundary the shop applies under its existing joint-area practice - and the caps stay on until the plates go into the furnace. Clean gloves are worn throughout; the treated faces are not handled bare-handed.
The batch was then coated in an Ir-Ta precursor system. The shop's furnace curve holds around 480℃ for a dozen minutes per pass, ten-odd passes to a plate, with a separate curve for mesh. At the time of filing, the racking check record had been filed under the batch number and the shift's furnace schedule was unchanged.
No Information