18
Nov, 2026
After the Flexible Anode Goes in the Trench
The back-and-forth before an order is usually about the anode itself — wire diameter, internal cable, coating, finished OD. Once the crates reach site, what decides whether the current spreads is a di
-
16
Nov, 2026
How to Specify an MMO Titanium Probe Anode for Internal Cathodic Protection
A cathodic protection probe anode solves one problem that tubular, wire, or flexible anodes cannot: internal corrosion in closed aqueous equipment. Where deep-well anodes go in soil and ribbon anodes
-
11
Nov, 2026
The Electrolyte Is Never Pure: How Impurities Quietly Spend Anode Life
Site electrolyte is rarely what the spec sheet says. Fluoride attacks the titanium under the coating, iron and lead scale up at mesh crossings, organics pack the cracks, and the lab's ALT report runs
-
09
Nov, 2026
Before the Cell: Anodes Age in the Warehouse
Most of the coating damage is already done by the time the crate is opened. Not in the cell.
-
04
Nov, 2026
10,000 Hours of Accelerated Life Is Not 10 Years in the Field
Why NACE TM0108 accelerated life hours cannot be read as field-year promises for MMO titanium anodes — and how to read an ALT report correctly.
-
02
Nov, 2026
Current Enters the Joint Before the Coating: Anode Contact Resistance
Why MMO titanium anode life depends on contact resistance and feed-point design, not just coating. Field notes on crimp joints, busbar bolts, and current taper.
-
28
Oct, 2026
Anode Geometry and Current Distribution: Why Cathode Matching Decides Field Life
The anode gets specified by coating. The cathode gets a line in the BOM. In the field, the first thing that goes wrong is usually neither.
-
26
Oct, 2026
Fluoride in the Electrolyte: Why the Coating Cannot Save the Titanium
A buyer once sent a drawing for an electro-oxidation tank and asked for "the usual Ir-Ta anode, like the last project." The last project was copper foil. This one was a fluoride-containing etchant rec
-
21
Oct, 2026
Probe Anode Through-Wall Installation: The Cable Seal Dies Before the Coating...
Through-wall probe anodes fail at the cable seal long before the MMO coating wears out. This article explains why resin canister potting, isolation length, and flow-induced cantilever motion decide re
-
19
Oct, 2026
Your Power Supply Is Part of the Anode System
MMO titanium anodes fail for reasons buyers rarely check: rectifier ripple, polarity reversal, dry start, wrong acid-wash sequence. Coating life depends on the power supply, not just the coating.
-
14
Oct, 2026
The Cathode Is Not Just the Other Plate
Buyers spec out anodes in exhausting detail: Ru-Ir or Ir-Ta, coating loading in g/m², Gr1 versus Gr2 substrate, rated life in years. The cathode gets a sentence, maybe. But in the field, when out
-
12
Oct, 2026
Same Anode, Different Life: What Operating Duty Explains That the Datasheet D...
Same part, same coating, same supplier — yet one cell runs for years and the other fails inside a season. The datasheet cannot explain this, because it describes the part, not the duty. This field not