How to Specify an MMO Titanium Probe Anode for Internal Cathodic Protection
Nov 16, 2026

Dr. Emily Carter
As a senior research scientist at Di Noer Technology, Dr. Carter specializes in the development of MMO noble metal mixed oxide coated titanium anodes. With over 15 years of experience in electrochemical materials, she leads the R&D team in creating innovative solutions for water treatment and energy storage industries.

A cathodic protection probe anode solves one problem that tubular, wire, or flexible anodes cannot: internal corrosion in closed aqueous equipment. Where deep-well anodes go in soil and ribbon anodes follow buried pipelines, a probe inserts directly into a heat exchanger water box, pressure vessel, or process tank from the outside. The cantilever design carries an MMO-coated titanium tip, an electrically isolated shaft section, and a cable exit on the dry side to the rectifier.
Why titanium substrate and MMO coating
Titanium Grade 1 or Grade 2 (ASTM B338 / ASTM B265) provides stiffness, passivity, and shape. The mixed metal oxide coating supplies electrocatalysis. In fresh water or low-chloride service, an iridium-tantalum (Ir-Ta) coating dominates oxygen evolution. In seawater, brine, or high-chloride condenser boxes, a ruthenium-iridium (Ru-Ir) coating evolves chlorine species that suppress biofouling alongside corrosion. Platinum on titanium is optional for high-purity or high-voltage duty but costs more and is sensitive to AC ripple. Lead alloys leach; graphite sheds. Titanium with MMO avoids those failure paths.
Current distribution and probe positioning
An internal probe protects roughly 2 to 3 pipe diameters along the bore before current density falls off. Probe spacing follows pipe diameter and flow geometry, not a fixed meter rule. In a water box or vessel, position the probe away from dead spots and away from the reference electrode. If the reference electrode sits next to the anode, the controller reads its own field and over-feeds.
Entry, isolation, and cable joint
The inactive shaft requires isolation from the shell using PVC, FRP, or PE decoupler. Entry options include threaded tank nozzle, flange nozzle, or hot-tap assembly for installation under pressure. The cable joint is crimped, covered with adhesive-lined heat shrink, and potted in resin, then pressure-tested before shipment. Design voltage above 8 V in chloride water risks titanium substrate passivation and breakdown.
Common failure modes engineers see
|
Failure mode
|
Cause
|
Prevention
|
|---|---|---|
|
Cable seal leak
|
Copper corrodes, open circuit
|
Resin canister + pressure test before shipment
|
|
Active coating too close to wall penetration
|
Shell polarizes, isolation fails
|
Maintain specified isolation length on inactive shaft
|
|
Probe bent by flow
|
Undersized rod diameter
|
Increase rod diameter or add supported shield
|
|
Reference electrode next to anode
|
System over-feeds itself
|
Separate probe and reference electrode by design distance
|
Typical specifications
|
Field
|
Typical value
|
|---|---|
|
Substrate
|
Titanium Gr1 / Gr2 / TA2 rod or tube
|
|
Active diameter
|
6 / 10 / 12.7 / 19 / 25 mm
|
|
Active length
|
100–300 mm (configurable)
|
|
Temperature
|
≤80 °C standard (higher on request)
|
|
Design life
|
Up to ~20 years under rated current, medium, and seal conditions
|
|
Entry
|
Threaded, flange, hot-tap
|
|
Decoupler
|
PVC / FRP / PE over inactive shaft
|
What you need to confirm before specifying
These fields cover the media named above; confirm chloride content, operating temperature, pressure, pipe or vessel diameter, target steel potential, and reference electrode type against your own operating conditions before you specify.
Di Noer Application Engineering Team · 2026 Nov 16